Red Terracotta Powdered Clay - 25kg
Temperature Range 1050øC - 1160øC
Shrinkage (w-d) 3 - 5%
Shrinkage (d-f) 8 - 10%
0.36% expansion at 500øC
Texture (1-smooth 10-coarse) 3 - 4.
Firedcolour- Red/ Brown.
Red Terracotta Casting Slip Recipe
P3102 Red Terracotta Clay - 50kg
Water - 19lt
P3342 Soda Ash - 100gm
P3344 Soda Sil - 240gm
Temperature Range 1050øC - 1160øC
Shrinkage (w-d) 3 - 5%
Shrinkage (d-f) 8 - 10%
0.36% expansion at 500øC
Texture (1-smooth 10-coarse) 3 - 4.
Firedcolour- Red/ Brown.
Red Terracotta Casting Slip Recipe
P3102 Red Terracotta Clay - 50kg
Water - 19lt
P3342 Soda Ash - 100gm
P3344 Soda Sil - 240gm
Firing Temperature | 1050-1160'c |
---|---|
Range | Earthenware/Terracotta |
Fired Colour | Red |
Texture | 4 - Medium |
Click on any of the following links to download the file.